What causes sink marks in injection - molded parts from an injection machine?

Jul 21, 2025Leave a message

Sink marks in injection-molded parts are a common yet frustrating issue that can significantly impact the quality and functionality of the final product. As a leading injection machine supplier, we understand the importance of addressing this problem to ensure our customers achieve the best results. In this blog, we will explore the various factors that cause sink marks in injection-molded parts and provide insights on how to mitigate them.

Material - related Causes

One of the primary factors contributing to sink marks is the material used in the injection molding process. Different plastics have varying shrinkage rates, and understanding these properties is crucial. For instance, semi - crystalline plastics such as polypropylene (PP) and polyethylene (PE) have relatively high shrinkage rates compared to amorphous plastics like polystyrene (PS) and polycarbonate (PC).

When semi - crystalline plastics cool, they undergo a phase change from a molten state to a solid crystalline structure. This phase change causes significant volume reduction, which can lead to sink marks. The molecular structure of these plastics allows for a more ordered packing of molecules during crystallization, resulting in a denser and smaller volume in the solid state.

Automatic Plastic Bottle Cap Injection Moulding Making Machine(001)Plastic Injection Moulding Machine 1(001)

Another material - related issue is the moisture content. If the plastic resin contains excessive moisture, it can cause problems during the injection molding process. When the molten plastic with high moisture content is injected into the mold, the water turns into steam. This steam can create voids and uneven cooling, leading to sink marks. It is essential to properly dry the plastic resin before use to prevent this issue.

Mold Design and Construction

The design and construction of the mold play a vital role in preventing sink marks. One key aspect is the wall thickness of the part. If the wall thickness is not uniform, thicker sections will cool more slowly than thinner ones. As the thicker sections cool and shrink, they pull on the surrounding material, creating sink marks on the surface. For example, in a part with a thick boss or rib connected to a thinner wall, the boss or rib will take longer to cool and can cause sink marks on the adjacent wall.

The gate design also affects the occurrence of sink marks. The gate is the opening through which the molten plastic enters the mold cavity. If the gate is too small, it can restrict the flow of plastic, leading to incomplete filling and uneven packing. On the other hand, if the gate is too large, it can cause excessive pressure and flow, resulting in over - packing in some areas and under - packing in others. A well - designed gate should ensure a balanced and smooth flow of plastic into the mold cavity.

The cooling system in the mold is another critical factor. An inefficient cooling system can lead to uneven cooling of the plastic part. If some areas of the mold are cooled too quickly while others are cooled too slowly, it can cause differential shrinkage and sink marks. The cooling channels should be properly designed and placed to ensure uniform cooling throughout the part. For example, in a complex mold, multiple cooling circuits may be required to achieve even cooling.

Injection Machine Settings

The settings of the injection machine also have a significant impact on sink marks. The injection pressure and speed are two important parameters. If the injection pressure is too low, the plastic may not be packed tightly enough in the mold cavity, resulting in shrinkage and sink marks. Conversely, if the injection pressure is too high, it can cause excessive stress on the plastic, leading to warping and sink marks in some cases.

The injection speed affects the filling time of the mold cavity. A slow injection speed may allow the plastic to start cooling before the mold is completely filled, resulting in uneven packing and sink marks. A fast injection speed, however, can cause turbulence and air entrapment, which can also lead to problems. It is necessary to find the optimal injection speed for each specific part and plastic material.

The holding pressure and time are also crucial. The holding pressure is applied after the mold is filled to maintain the pressure and ensure proper packing of the plastic. If the holding pressure is too low or the holding time is too short, the plastic will not be adequately packed, and sink marks may occur. On the other hand, if the holding pressure is too high or the holding time is too long, it can cause excessive stress and flash.

Process Conditions

The process conditions, such as the melt temperature and the mold temperature, can also contribute to sink marks. The melt temperature affects the viscosity of the plastic. If the melt temperature is too low, the plastic may be too viscous to flow easily, leading to incomplete filling and sink marks. If the melt temperature is too high, it can cause degradation of the plastic and uneven cooling, resulting in sink marks.

The mold temperature also plays an important role. A low mold temperature can cause the plastic to solidify too quickly, especially in the surface layer. This can prevent proper packing and lead to sink marks. A high mold temperature, on the other hand, can slow down the cooling process and may cause warping and other issues. It is necessary to maintain an appropriate mold temperature for the specific plastic material and part design.

Solutions and Mitigation Strategies

To address the issue of sink marks, several solutions can be implemented. In terms of material selection, choose plastics with lower shrinkage rates if possible. For semi - crystalline plastics, consider using additives or blends that can reduce the shrinkage. Also, ensure proper drying of the plastic resin to eliminate moisture.

For mold design, strive for uniform wall thickness. If it is necessary to have thick sections, use internal ribs or bosses with a more gradual transition to the thinner walls. Optimize the gate design to ensure a balanced flow of plastic. Additionally, improve the cooling system by adding more cooling channels or adjusting their layout to achieve uniform cooling.

On the injection machine side, adjust the injection pressure, speed, holding pressure, and time to ensure proper filling and packing of the plastic. Monitor and control the melt temperature and mold temperature to maintain optimal process conditions.

Our Injection Machines and Solutions

At our company, we offer a wide range of high - quality injection machines that are designed to minimize the occurrence of sink marks. Our Automatic Plastic Bottle Cap Injection Moulding Making Machine is equipped with advanced technology to ensure precise control of the injection process. It can handle different types of plastic resins and produce high - quality bottle caps with minimal sink marks.

Our PET Plastics Injection Molding Machine is specifically designed for PET plastics. It has features such as accurate temperature control and optimized injection parameters to prevent sink marks in PET parts.

The Plastic Injection Moulding Machine in our product line is a versatile machine that can be used for various plastic injection molding applications. It offers flexibility in terms of mold design and process settings, allowing our customers to achieve the best results and reduce the occurrence of sink marks.

If you are facing issues with sink marks in your injection - molded parts or are looking for a reliable injection machine supplier, we invite you to contact us for a detailed discussion. Our team of experts can provide you with customized solutions based on your specific requirements.

References

  1. Throne, J. L. (1996). Plastics Process Engineering. Hanser Publishers.
  2. Rosato, D. V., & Rosato, D. V. (2000). Injection Molding Handbook. Kluwer Academic Publishers.
  3. Beecher, J. F. (2003). Injection Molding for Medical and Electronic Applications. Society of Plastics Engineers.
Send Inquiry